Please can someone advise on the best epoxy to use for pressure sealing?
I am trying to seal a cavity on top of an RF filter which contains the tuning screws. The unit is pressurised to 3.5bar and the leak rate has to be better that 5cc/hr.
We have tried eccobond type epoxies, but after aging it begins to leak around the ends of the epoxy seal.
I think that the epoxy is not sticking properly to the filter housing (aluminium, painted with two part black epoxy paint).
We have tried stripping the paint off to leave bare metal but the epoxy still seems to leak at the edges as if it has crept away.
I don't think we are using the right epoxies (eccobond and the like are adhesives or used for encapsulating components, not for pressure sealing).
Any suggestions?
I am trying to seal a cavity on top of an RF filter which contains the tuning screws. The unit is pressurised to 3.5bar and the leak rate has to be better that 5cc/hr.
We have tried eccobond type epoxies, but after aging it begins to leak around the ends of the epoxy seal.
I think that the epoxy is not sticking properly to the filter housing (aluminium, painted with two part black epoxy paint).
We have tried stripping the paint off to leave bare metal but the epoxy still seems to leak at the edges as if it has crept away.
I don't think we are using the right epoxies (eccobond and the like are adhesives or used for encapsulating components, not for pressure sealing).
Any suggestions?