Apr 16, 2015 #1 FMSArg Materials Joined Jan 12, 2011 Messages 3 Location AR Hi, I´m working in a company that produces filament wound anhydride epoxy-fiberglass pipes. I have to develop a line with aromatic amine epoxy. For occupational safety issues I seek out a epoxy system MDA free. Could you help me?
Hi, I´m working in a company that produces filament wound anhydride epoxy-fiberglass pipes. I have to develop a line with aromatic amine epoxy. For occupational safety issues I seek out a epoxy system MDA free. Could you help me?
Apr 16, 2015 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US There are aliphatic amines, like DETA, that can be used as the curing agent/hardener for epoxy resins.
There are aliphatic amines, like DETA, that can be used as the curing agent/hardener for epoxy resins.
Apr 16, 2015 Thread starter #3 FMSArg Materials Joined Jan 12, 2011 Messages 3 Location AR Hi CoryPad, the pipes have a long-term hydrostatic strength requirements (water and temperature). Aliphatic and cycloaliphatic amines systems do not perform as well as aromatic amines
Hi CoryPad, the pipes have a long-term hydrostatic strength requirements (water and temperature). Aliphatic and cycloaliphatic amines systems do not perform as well as aromatic amines
Apr 17, 2015 #4 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US So you want to use an aromatic amine hardener, but not MDA? I would contact Dow and Huntsman for suitable products.
So you want to use an aromatic amine hardener, but not MDA? I would contact Dow and Huntsman for suitable products.
Apr 20, 2015 Thread starter #5 FMSArg Materials Joined Jan 12, 2011 Messages 3 Location AR Thanks CoryPad