We have recently changed from water disinfection by chlorine gas to chlorine dioxide. Previously specified seals and gaskets to be manufactured from EPDM. It has been suggested by one manufacturer that EPDM is no longer suitable for use with chlorine dioxide disinfectant and that we should change our specification for seals and gaskets to Flourocarbon (FKM) Rubber.
We need a material that is suitable for use in water service with both chlorine and chlorine dioxide disinfectants.