EPDM to EPDM adhesive?

Status
Not open for further replies.

Hercules28

Materials
Nov 9, 2010
169
For water applications. No Silicon.

Any ideas?

Open to anything regarding how to apply..Injection molding - Caulk guns ....

Thanks,

Herc
 
Replies continue below

Recommended for you

Vulcanisation of the two parts with the aid of fe chemosil 6025 and a solution of the same EPDM. Afterwards thorough cleaning of the part?

I'm not an expert to (drinking) water regulations .
 