Feb 13, 2020 1 #1 faizal1306 Materials Joined Feb 13, 2020 Messages 1 Location MY how to improve epdm hot tear problem that causing part easy to crack during demolding?
Mar 14, 2020 #2 Alexandr36484 Chemical Joined Jul 18, 2016 Messages 8 Location UA The introduction of PP will increase physical and mechanical properties Upvote 0 Downvote
May 6, 2020 #3 Violka Chemical Joined Nov 21, 2011 Messages 4 Location IL replace a small amount of CB with precipitated silica, about 5-10 phr Upvote 0 Downvote