Jul 10, 2012 #1 MoCoWiTx Structural Joined Jul 10, 2012 Messages 1 Location US Can anyone point me to a chart for the engineering properties for (used) drill stem that is utilized as columns in agricultural buildings? Thanks, MoCOWiTx
Can anyone point me to a chart for the engineering properties for (used) drill stem that is utilized as columns in agricultural buildings? Thanks, MoCOWiTx
Jul 17, 2012 #2 boo1 Mechanical Joined Oct 31, 2001 Messages 2,129 Location US API Spec 7, Specification for Rotary Drill Stem Elements, Fortieth Edition, the grade will determine the properties. Specification for Rotary Drill Stem Elements ANSI/API SPECIFICATION 7-1 FIRST EDITION, MARCH 2006 is attached http://files.engineering.com/getfile.aspx?folder=a8e3a2aa-3b45-46ed-95ef-1cf0214646b3&file=7_1_addn_022807.pdf Upvote 0 Downvote
API Spec 7, Specification for Rotary Drill Stem Elements, Fortieth Edition, the grade will determine the properties. Specification for Rotary Drill Stem Elements ANSI/API SPECIFICATION 7-1 FIRST EDITION, MARCH 2006 is attached