Apr 27, 2005 #1 rmetzger Mechanical Joined Dec 2, 2004 Messages 200 Location US 1080 seems to be mentioned quite a bit but I've found no conclusive evidence. Anyone?
Apr 27, 2005 #2 codeeng Petroleum Joined Feb 9, 2004 Messages 365 Location CA SAE1074, 1075 and 1080 are considered alternative grades per this link: http://www.ameri-source.com/carbon_steel_strips/stan.html Upvote 0 Downvote
SAE1074, 1075 and 1080 are considered alternative grades per this link: http://www.ameri-source.com/carbon_steel_strips/stan.html