Hi All, I have a materials question with regards to the EN 13480 code. We can't get round bar in the diameter we require in P355 to make a tube with flanges on the end. The flanges have already been manufactured in P355. Is it permissible under the EN 13480 code to weld Stainless steel to Carbon steel? it'll either be 304/316 (1.4307 or 1.4401)?
Thanks for any help