Oct 9, 2006 #1 teran Materials Joined Jun 29, 2006 Messages 9 Location KR The EN10160(Ultrasonic Examination), Can be applicable to austenite & austenoferritic(Duplex)?
Oct 11, 2006 #2 ijzer Materials Joined Oct 25, 2002 Messages 313 Location NL According to the index/scope of EN 10160 is it is not for austenitic and duplex steels. Upvote 0 Downvote