Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

En equivalent AISI standard material datas

Status
Not open for further replies.

heavenly

Aerospace
Joined
Dec 30, 2004
Messages
38
Location
IN
Hi,
I am looking for En8 equivalent materials from AISI standard.How to get these details through internet resources

Thanks in before

John
 
Go to MatWeb Search for EN8, and find AISI 1040 Steel, available with various heat & mechnical treatment. One specific example:
"AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 100 mm (4 in.) round
...
Key Words: UNS G10400, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A546, ASTM A576, ASTM A682, MIL SPEC MIL-S-11310 (CS1040), SAE J403, SAE J412, SAE J414, DIN 1.1186, JIS S 40 C, BS 970 060A40, BS 970 080A40, BS 970 080M40 (EN8), BS 2 S 93"


Composition & properties are given, & sometimes supplier links.
 