Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Embedding Aluminium insert during lamination process

Status
Not open for further replies.

NPC9092

Aerospace
Jan 13, 2020
1
Hey, I have a component for which I need to embed some aluminium inserts into a CFRP component during the laminating procedure.

The part consists of a foam core wrapped in carbon. The aluminium inserts are for the connection points.

I was wondering if you could help me with some tips about making a reliable bond between the inserts and the carbon layers.
I have the following plan:
-Sandblast the inserts to obtain a rough surface and remove the oxide layer,
-Treat the surface with 3M AC130 surface pre-treatment,
-Coat inserts with resin to insulate from carbon fibers (avoid galvanic cell),
-Perform lamination (hand laminate)

Please let me know if there is anything that I'm missing.
 
Replies continue below

Recommended for you

Speaking off-hand, its generally poor practice to install aluminum alloys in carbon-fiber structures for many reasons... unless this is a 'throw-away' space part.

Small size of aluminum pieces VS large mass of carbon is almost assuredly a high corrosion potential 'fight' for any finish that is thin/failed/missing [IE: bare hole].

Carbon fiber and aluminum stiffness mismatch... load strain and thermal strain... could lead to disbonds.

Perhaps You should consider titanium 6AL-4V annealed or 15-5PH CRES H1025-to-H1100... lightly grit blasted and silane coated [or Sol-Gel AC130-variant, etc].



Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 