What type of silicone rubber and/or additive would give/increase the elongation % to as much as 400-500%? Any idea/help is appreciated.
 
Replies continue below

Recommended for you

It's best to start with a polymer that will achieve that type of a property. Check with the manufacturer prior to purchasing.
 