Hi could anyone provide an example of chloride corrosion on austenitic stainless steel shown on the ellingham diagram please?
 
Replies continue below

Recommended for you

Sounds like a homework question- student posting is not permitted- against forum rules. Though as a homework question its bizarre- the corrosion reactions are too complicated to isolate as a simple Elligham diagram and plain meaningless as it is kinectics that matter.
 
Thank you MH97

I was simply going to answer 'yes'.

= = = = = = = = = = = = = = = = = = = =