Hi,

I am trying to find data on electropolished steels (emissivity, etc.) Can anybody please point me to a proper resource page?

Thanx a bunch,

DAS
 
Replies continue below

Recommended for you

Yes, I have tried it. No good, though. I'll keep looking. Thanks.

DAS
 
Are you expected the emissivity to be radically different than the 0.11 given in the table?

TTFN
 
No, I do not. This number is as good as any other, huh? At least a reference number. I appreciate the help.
 
That value seems pretty consistent with the value for polished nickel at 0.07.

Even polished aluminum is listed at 0.04 to 0.06.

TTFN
 