we've just welded up some mild steel flanges (1018/1020) to an A53 pipe, then electroless nickel plated the assembly.
small cracks have been noted in the final piece and questions are arising as to whether it was the welding process that created the cracks, or the post-weld plating.
has anyone ever experienced weld cracking as a result of applying electroless nickel?
these parts were heat treated to stress relieve the welds prior to nickel plating.
CS
small cracks have been noted in the final piece and questions are arising as to whether it was the welding process that created the cracks, or the post-weld plating.
has anyone ever experienced weld cracking as a result of applying electroless nickel?
these parts were heat treated to stress relieve the welds prior to nickel plating.
CS