Electrically Insulative Coating for Steel?

Status
Not open for further replies.

ajensen

Mechanical
Mar 4, 2011
22
Hi,

I have a small stainless part (think washer, but irregularly shaped) that is about .250" in diameter and between .005" and .010" thick. The part holds a mating piece in position and is designed with fairly tight tolerances (+/- .001" around the profile). I need to electrically insulate this part and am wondering if there is a very thin coating/plating (less than .001") that will do the job. Does anyone have suggestions for a process that might work? Keep in mind the final part dimensions still need to be held to within +/-.001" so whatever coating/plating process is used must be accurate and repeatable enough so that the post-coated/plated dimensions are in spec. The coating/plating does not need to be a super insulator as we are only dealing with less than 4V and less than 600mA.

 
Replies continue below

Recommended for you

What voltage must be resisted?

0.001 thickness of anything will prevent very, very little voltage. Worse, it can too easily be scratched through, nicked, sliced etc during assembly/re-assembly/repair and lose any resistance.

Make the whole thing of your plastic. As a locator of the next part and not a retainer or bolt or prying point of stress, you'll see only minor pressures that can easily be withstood across such a small distance.
 
ajensen,

If you need a hard, accurate, non-conductive washer, how about some sort of machinable ceramic?

Ask your machine shop what they like.

Critter.gif
JHG
 
paralene is a good insulator but is easily scratched and is usually only about 0.0001" thick

MACOR is an excellent machinable ceramic but would be subject to fracture if subject to any bending - meaning the mating surfaces must be flat
 