Hi Everybody,
I am doing some experimental work on hole cold expansion and have measured the strains around a cold expanded hole. I have full field principal strains around the cold expanded hole and would like to convert these strains to stresses.
I am looking for a clear analytical (i.e I don't want to put the data into Abaqus, Nastran etc.) algorithm or method to convert the plastic strains to stresses.
I have having a hard time finding clear information on how to do this so any advice, tips etc would be helpful.
Thanks in advance,
Dave
I am doing some experimental work on hole cold expansion and have measured the strains around a cold expanded hole. I have full field principal strains around the cold expanded hole and would like to convert these strains to stresses.
I am looking for a clear analytical (i.e I don't want to put the data into Abaqus, Nastran etc.) algorithm or method to convert the plastic strains to stresses.
I have having a hard time finding clear information on how to do this so any advice, tips etc would be helpful.
Thanks in advance,
Dave