Hello,

I am designing a piston cylinder with a moblie elastomer (nylon with neoprene coating) diaphragm seal that moves with the piston.

How do I go about determining the travel of the diaphragm before failure of the elastomer?

Your help would be greatly appreciated.

ADNPD

 
Replies continue below

Recommended for you

Make the diaphram into a ROLLING diaphram. Essentially stress free.
 