nicolasdegand
Mechanical
Hi,
I'd like to use an elastic-plastic material. I define as
-elastic: young modulus and poisson's ratio (217460 N/mm2 and 0,298)
-plastic:yield stress and plastic strain (258N/mm2 and 0)
But I'd like to extract the values as elasto-plastic behaviour so define the gradient of the tangent of the curve in the plastic behaviour. So, to have a linear behaviour until the yield stress and than a gradient of 3% of the young modulus in the plastic part.
How to do?
I tried to define in "plastic">suboptions>rate dependent>hardening>yiel ratio>
Yield stress ratio Eq plastic strain rate
258 0
300 6500 (+/-3% of E)
But it doesn't work!
Thanks a lot,
Nico
I'd like to use an elastic-plastic material. I define as
-elastic: young modulus and poisson's ratio (217460 N/mm2 and 0,298)
-plastic:yield stress and plastic strain (258N/mm2 and 0)
But I'd like to extract the values as elasto-plastic behaviour so define the gradient of the tangent of the curve in the plastic behaviour. So, to have a linear behaviour until the yield stress and than a gradient of 3% of the young modulus in the plastic part.
How to do?
I tried to define in "plastic">suboptions>rate dependent>hardening>yiel ratio>
Yield stress ratio Eq plastic strain rate
258 0
300 6500 (+/-3% of E)
But it doesn't work!
Thanks a lot,
Nico