if you could send me the type of wood that you are looking for i have a good source on here at my desk which will list the properties that you might be looking for....for example:
American White Oak
Data is based on small, clear, air-dried samples unless specified.
PHYSICAL PROPERTIES
Density, g/cc 0.68 0.68 g/cc
MECHANICAL PROPERTIES
Tensile Strength, Ultimate, MPa 5.5 transverse. 798 psi
Flexural Modulus, GPa 12.4 12.28-12.4 GPa in bending; 0.105 GPa Modulus of rupture in bending. 1,798 ksi
Flexural Yield Strength, MPa 56.5 MPa bending stress at proportional limit. 8,195 psi
Compressive Yield Strength, MPa 50 48.3-51 MPa axial (parallel to grain); 9.1 MPa transverse. 7,252 psi
Shear Strength, MPa 13.5 13.1-13.8 MPa 1,958 psi
CTE, linear 20ºC, µm/m-°C 4.9 axial. Typical value for Oak. 2.7 µin/in-°F
CTE, linear 20ºC Transverse to Flow, µm/m-°C 11.1 radial; 54.4 µm/m-°C tangential. Typical values for Oak. 6.2 µin/in-°F