Our Pipeline Details are 219.1 mm OD, WT 7.04 mm CA=3mm, DP 70 barg Tdesign = 83 deg and T min = -5 deg c. Pipe material API 5L X60
Based on the above The minimum elastic bending radius calculated is 250 m. However, if I use the WT as 6.35 mm the minimum elastic bending radius required is 360 m. But the same 360 m if we uses in the Hydrotest calculation, the equivalent stress criteria fails where as with WT 7.04 mm it satisfies the criteria .
If we increase the min bend radius in 6.35 mm from 360 m to 4000 m it satisfies the equivalent stress criteria. Does this is alloweed to increase the bend radius to 4000 m?
Our Pipeline Details are 219.1 mm OD, WT 7.04 mm CA=3mm, DP 70 barg Tdesign = 83 deg and T min = -5 deg c. Pipe material API 5L X60
Based on the above The minimum elastic bending radius calculated is 250 m. However, if I use the WT as 6.35 mm the minimum elastic bending radius required is 360 m. But the same 360 m if we uses in the Hydrotest calculation, the equivalent stress criteria fails where as with WT 7.04 mm it satisfies the criteria .
If we increase the min bend radius in 6.35 mm from 360 m to 4000 m it satisfies the equivalent stress criteria. Does this is alloweed to increase the bend radius to 4000 m?