Does anyone out there know of any research on the effect of temperature on the material properties of Manganese Bronze C67500?

I need to know what the tensile and yield strengths would be around 500F. I also need to know if the material would be useful at all around this temperature.
 
Replies continue below

Recommended for you

I used to work with some of the cast grades of MnBronze. As I recall there is published data in the ASM Handbook up to 450F. I think that even for the high strength grades you will find the strength at temp to be around 5ksi. Above about 300F it drops quickly.

= = = = = = = = = = = = = = = = = = = =
Still trying to help you stop corrosion.
formerly Trent Tube, now Plymouth Tube
eblessman@plymouth.com
or edstainless@earthlink.net
 