I am having difficulty hardening a CA15 casting. The chemistry is within the ASTM spec including the trace elements. The heat treatment I have been running has worked on different lots with similar composition. 1850F - 3h Fan cool usually results in close to 400BHN hardness. On this lot the hardness the first time around was 280BHN, after running the same cycle it dropped to 250 BHN and after running the same cycle third time it dropped down to 200BHN.
I am trying to understand the reason for the hardness to drop after consecutive normalize cycles.
Also is there any way I can regain the 400BHN hardness on this casting?
Please comment.
Thank you
Mahadhatu
I am trying to understand the reason for the hardness to drop after consecutive normalize cycles.
Also is there any way I can regain the 400BHN hardness on this casting?
Please comment.
Thank you
Mahadhatu