Hi Folk! Good Day!
This is regarding the 2:1 Ellipsoidal dish EFE & end heat treatment, dish end nominal thickness is 20mm and material is SA-516 Gr. 70 N.
As per the code clause UCS-79 (d) is applicable, which states “if dish end formed with cold forming and determined the extreme fiber elongation(EFE) higher than 5% then heat treatment shall be performed as per UCS-56 temperature & holding time”
But over and above, client specification of SHELL DEP is also applicable, which states that “in case of dish end cold formed and determined the EFE higher than 5% then NORMILIZING shall be performed with following temperature (850 to 960 deg C)”
As per UCS-56:
Dish end Nominal thickness = 20mm
Holding minimum Temperature shall be = 595 Deg C.
Holding minimum time duration = 1 Hr / 25mm
Holding minimum time duration per mm = 2.4 minute / mm
Now as per Nominal thickness holding time = 20 x 2.4 => = 48 minute.
As per Shell DEP:
Holding Temperature shall be = 850 to 960 Deg C
Holding minimum time duration = Need to specify, as SHELL DEP is silent on Holding time.
Question no-1 : Whether Holding time for normalizing shall be followed as per UCS-56 or as per material test report (MTC)?
If we see on material test report, it is calling for 1.75 minute / mm and if we calculate as per MTR then it shall be 1.75 x 20 = 35minute.
Question no-2 : Please advice material specialized person & vessel design engineers on above clarification. that what can be the effect on original material properties due to higher holding time considering for normalizing.
This is regarding the 2:1 Ellipsoidal dish EFE & end heat treatment, dish end nominal thickness is 20mm and material is SA-516 Gr. 70 N.
As per the code clause UCS-79 (d) is applicable, which states “if dish end formed with cold forming and determined the extreme fiber elongation(EFE) higher than 5% then heat treatment shall be performed as per UCS-56 temperature & holding time”
But over and above, client specification of SHELL DEP is also applicable, which states that “in case of dish end cold formed and determined the EFE higher than 5% then NORMILIZING shall be performed with following temperature (850 to 960 deg C)”
As per UCS-56:
Dish end Nominal thickness = 20mm
Holding minimum Temperature shall be = 595 Deg C.
Holding minimum time duration = 1 Hr / 25mm
Holding minimum time duration per mm = 2.4 minute / mm
Now as per Nominal thickness holding time = 20 x 2.4 => = 48 minute.
As per Shell DEP:
Holding Temperature shall be = 850 to 960 Deg C
Holding minimum time duration = Need to specify, as SHELL DEP is silent on Holding time.
Question no-1 : Whether Holding time for normalizing shall be followed as per UCS-56 or as per material test report (MTC)?
If we see on material test report, it is calling for 1.75 minute / mm and if we calculate as per MTR then it shall be 1.75 x 20 = 35minute.
Question no-2 : Please advice material specialized person & vessel design engineers on above clarification. that what can be the effect on original material properties due to higher holding time considering for normalizing.