Dear all,

We have an US vessel supplier refuses to comply with EEMUA 190 for material properties and test requirements after purchase order already placed. Before PO, they did confirm they will comply.
What their claim is: plant is in US, so only need to comply with ASME Div.1 requirements for material and testing.

EEMUA has more requirements than ASME code on carbon equivalent, UT, impact test, hardness test. For mounded bullet buried under soil and sand, and for plant in US, is EEMUA 190 mandatory ? Will only ASME Div. 1 be sufficient ? Thanks for you opinion.
 