Jun 25, 2004 #1 mtcf New member Joined Jun 25, 2004 Messages 1 Location US I am looking for an equivalent "American" steel for 070M20. Does anyone have any info? Thanks for your help Calinic
I am looking for an equivalent "American" steel for 070M20. Does anyone have any info? Thanks for your help Calinic
Jun 25, 2004 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US SAE 1021 Upvote 0 Downvote