Hello,
I need some clarifications about below paragraph. I appreciate if you can help me.
1. What does quaranteed minimum value mean ? S-basis allowable ?
2. “premium selection” of the material ? Does it mean a single test of particular raw material to be used in design.
3. If I test the raw material (exact heat only) and use that values, I dont need to generate statisc based allowables.
"(e) Design values greater than the guaranteed
minimum’s required by this paragraph may be
used where only guaranteed minimum values are
normally allowed if a “premium selection” of the
material is made in which a specimen of each
individual item is tested before use to determine
that the actual strength properties of the particular
item will equal or exceed those used in design."
Thanks and Regards
I need some clarifications about below paragraph. I appreciate if you can help me.
1. What does quaranteed minimum value mean ? S-basis allowable ?
2. “premium selection” of the material ? Does it mean a single test of particular raw material to be used in design.
3. If I test the raw material (exact heat only) and use that values, I dont need to generate statisc based allowables.
"(e) Design values greater than the guaranteed
minimum’s required by this paragraph may be
used where only guaranteed minimum values are
normally allowed if a “premium selection” of the
material is made in which a specimen of each
individual item is tested before use to determine
that the actual strength properties of the particular
item will equal or exceed those used in design."