Dear Experts;

What is the difference between E7018 and E7018M as per ASME Sec II Part C.



M.FAHAD RANA
WELDING ENGINEER
 
Replies continue below

Recommended for you

The M is for the Metric / SI version of the spec.
 
M often denotes military grade. There are many differences in the two...including CVN test temp. Suggest you open the Code to see.
 
Agree 100% with David regards actually opening the code.
If you are a Welding Engineer you should not be asking these questions on an internet forum.
 