Nov 27, 2019 #1 FAHADRANA Mechanical Joined Nov 14, 2019 Messages 4 Location PK Dear Experts; What is the difference between E7018 and E7018M as per ASME Sec II Part C. M.FAHAD RANA WELDING ENGINEER
Dear Experts; What is the difference between E7018 and E7018M as per ASME Sec II Part C. M.FAHAD RANA WELDING ENGINEER
Nov 27, 2019 #2 Geoff13 Structural Joined Oct 2, 2018 Messages 477 Location CA The M is for the Metric / SI version of the spec. Upvote 0 Downvote
Nov 27, 2019 #3 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA M often denotes military grade. There are many differences in the two...including CVN test temp. Suggest you open the Code to see. Upvote 0 Downvote
M often denotes military grade. There are many differences in the two...including CVN test temp. Suggest you open the Code to see.
Nov 28, 2019 #4 DekDee Petroleum Joined Mar 12, 2012 Messages 1,323 Location PH Agree 100% with David regards actually opening the code. If you are a Welding Engineer you should not be asking these questions on an internet forum. Upvote 0 Downvote
Agree 100% with David regards actually opening the code. If you are a Welding Engineer you should not be asking these questions on an internet forum.