Hello All,

I am working with a foundry in China and I am having difficulty settling on a lead-free alloy.
The casting is for use in a coffee machine and so must be lead-free, have good corrosion resistance to the mild saline water from the water softener and to the coffee acids at the operating temperature (170-200F). There is also significant secondary machining so a reasonable machinability rating would be preferable.

The alloy that I initially specified is a silicon bronze - C87850 but the foundry cannot supply it at a reasonable cost and suggest substituting H85 (which I presume is C23000) or H68As (presumably C26800 with Arsenic, although none is listed in the composition).

H85 Composition: Cu 84-86 Ni 0.5 Fe 0.1 Pb 0.03 Zn (balance) other 0.3
H68As Composition: Cu 67-70 Zn (balance) Pb 0.03 P 0.01 Fe 0.1 Sb 0.005 Bi 0.002 other 0.3
[single values are maximums]

Both of these specifications however are for wrought brasses and I can find no information about their casting properties. If the part can be cast from C23000 and the factory can perform the secondary machining, then I see no objections. However, I have so far failed to find any information about casting this alloy.

Any light shed on this would be greatly appreciated.

Many thanks,

Token
 
Have you looked at alloys on Copper.org?
Often you can look up a wrought alloy and casting equivalent.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Hi EdStainless,

Thanks for the response.
I have spent quite a few hours on copper.org and have not come across a way of finding cast equivalents to wrought products. I tried the advanced search feature by chemical composition (which helpfully doesn't allow searched by either copper or zinc content) but couldn't find anything.

Many thanks,

Token
 
@token
You could send a mail to copper.org, and they shall respond, with adequate literature or research reports. I have benefitted from them.


"Even,if you are a minority of one, truth is the truth."

Mahatma Gandhi.
 
Thanks arunmrao,

I will send them a mail.

 