I would agree with gerhardl. The other option may be, assuming that the valve is screwed 800#, go with a 1500# rated or 4000 psi. Similarly it is almost never feasible to look at overlay on such a small valve.
However my real reason for bothering to type is: 3mm corrosion allowance on a 3/4" line?? And, as I have commented before, with that level of corrosion in a valve it will have long since ceased operating as a valve, it will just be an expensive orifice. I appreciate that many valves are installed and left open, but really, good practice would dictate that all valves should be tested for operability on a regular basis and once you have significant corrosion I suggest that you will find this during such a test.