Hi all

Does anyone out there have any experience with operating flowlines using 8" DUX DCV-C600 series choke valves? We have had an issue with the flow being directed to the side wall of the valve & downstream flowline when operating the valve at less than 40% open & am just lookin to see if anyone else has had a similar experience.

Thanks
Jim
 
Replies continue below

Recommended for you

hsbcn

We are in contact with DUX, but just wanted to put feelers out through industry to see if any others used these valves and what their experience had been.
 
Hi Jim,
I am new to this forum, as you will see from my e-mail, i work for Duxvalves in the UK.
If you are experiencing any issues with our valves, i would welcome the chance to meet with you and get resolved.
Kind regards,
Dominic Clarke
 
Ask Dux about the Apache - North Sea application where they solved a major errosion problem.
 