It depends on the duplex SS and the environment.
The duplex SSs are significantly less susceptible to chloride SCC than the austenitic, 300-series, SSs. The alloy manufacturers such as Avesta-Sheffield, Usinor, Sandvik, VDM, etc. have tons of comparative information to help you decide which duplex SS is the solution to a problem with SCC of austenitic SS. Even the duplex SSs have a ladder of performance depending on their Cr and Mo contents. This puts Ferralium 255 and 2507 ahead of 2205, with 2304 coming lower than 2205 in chloride pitting and SCC resistance. Conversely, if the SCC is from hot caustic solutions, the 2304 may be superior to 2205.
In other words, there is no simple answer. But one thing is sure: duplex SSs are less susceptible to CSCC than the 300-series austentic SSs.