Dear Friends
I was asked to prepare WPS for Duplex Stainless Steel varies from 1" to 8" x Min Thks 5mm to 38mm.
Impact Value -40 deg celcius
Process - ROOT and Hot pass - GTAW / Fill & Cap-SMAW
Pls guide me in preparing Proposed WPS complyimng to ASME Sect IX-QW-403.6 & QW-451
Thanks
I was asked to prepare WPS for Duplex Stainless Steel varies from 1" to 8" x Min Thks 5mm to 38mm.
Impact Value -40 deg celcius
Process - ROOT and Hot pass - GTAW / Fill & Cap-SMAW
Pls guide me in preparing Proposed WPS complyimng to ASME Sect IX-QW-403.6 & QW-451