Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Duplex SS - grade 1

Status
Not open for further replies.

jam69

Chemical
Dec 24, 2002
1
Dear All,
I am not a expert in this field but, in certain extend, my work do requires me to endevour into this field. Can any of our fellow experts explain to me the difference between
Duplex SS ASTM A790 UNS S31803 and Duplex SS ASTM A790 CD3MWCuN in term of chemical composition, physical properties and commercial value

Your input is greatly appreciated.


Thank you.
 
Replies continue below

Recommended for you

A790 is "Standard specification for Seamless and Welded Austenitic Stainless Pipe", and contains UNS 31803, which is commonly called 2205. For lots of information on this alloy, see a manufacturers web page, such as
CD3MWCuN is a cast grade of stainless steel commonly called Zeron 100. It is not referenced in A790 since those are wrought material. It is listed in A890 as Gr. 6A (UNS J93380).
 