Duplex SS Charpy Impact Value conversion

Status
Not open for further replies.

WeldingPartner

Industrial
Apr 5, 2004
12
Hello,
Is there a formula with which you can convert Charpy impact values of a given duplex ss testpiece to impact values @lower temp (same wallthickness/ same weldingprocess etc), thus avoiding the need for retests. Thanks in advance.
WeldingPartner
 
Replies continue below

Recommended for you

No, actual impact tests must be performed at lower test temperatures.
 
You can correct for sample size but not temp.
You must do the real thing.

= = = = = = = = = = = = = = = = = = = =