Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Duplex 2205 Friction 1

Status
Not open for further replies.

DRW75

Structural
Oct 14, 2004
89
Hey folks,

(not sure if this is the correct forum but...)

Does anyone have friction coefficients for duplex 2205 on duplex 2205?

I suspect that I am going to have to run a few tests to determine it, but some preliminary guidance would be nice.

thanks

DRW

 
Replies continue below

Recommended for you

DRW75

A Google search for 2205 duplex ss revealed 0.3-0.5 for the coefficient of friction under dry conditions. I would run your own tests to be sure.
 
metengr, you must be the king wizard of google searching. i wansnt able to find that at all when i tried.

thanks