What is the minimum required support for a sanitary sewer ditch crossing?
We have a 15' (at bottom with sideslopes of 2:1) ditch crossing with a 8" DIP sewer main. What concerns do I need to look check...hydraulics of stream or scour, pipe supports detail, length of pipe exposed prior to support, corrosion protection, ???
Site is in Southeast and freeze not a major concern. We could raise the sewer main from 1' above bottom, but can not lower (due to recieving manhole invert).
We have a 15' (at bottom with sideslopes of 2:1) ditch crossing with a 8" DIP sewer main. What concerns do I need to look check...hydraulics of stream or scour, pipe supports detail, length of pipe exposed prior to support, corrosion protection, ???