Can I get some help please in obtaining/calculating values to input for FRACTURE STRAIN, STRESS TRIAXILITY and STRAIN RATE within the Damage for Ductile Metals material behaviour please?

I have seen the Hooputra documentation, I am still confused.

Thanks in advance
 
Replies continue below

Recommended for you

They can be obtained for particular material from experiments or from research papers.

Check the article "Identification of Ductile Damage Parameters" by Prantl et al. for reference.
 
Hi FEA way, I have no experimental data. My dissertation is purely numerical.

I have stress strain curves that I have converted to True and applied to the plastic properties, is there a way to determine the values in question using those figures? i.e. yield stress and plastic strain?
 