Hi engineers , I want to add ductile damage to a problem (compression test) but I'm not sure about inputs. here's what I'm thinking :
fracture strain (0.024886539) is obtained from plastic-strain plot (last strain before breaking of the test sample)
stress triaxiality considered (0)zero
strain rate is considered (1) because it doesn't affect the simulation (strain rate not important )
but I'm not sure about "Displacements at failure", what should I insert?
fracture strain (0.024886539) is obtained from plastic-strain plot (last strain before breaking of the test sample)
stress triaxiality considered (0)zero
strain rate is considered (1) because it doesn't affect the simulation (strain rate not important )
but I'm not sure about "Displacements at failure", what should I insert?