Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Dual certified fittings

Status
Not open for further replies.

DVNMech

Mechanical
Jan 18, 2005
9
Hi,

Is it common to order dual certified stainless steel fittings and pipe (304/304L) to benefit of the properties of both materials? Or is there a higher probability that such pipe/fittings can't be delivered?
 
Replies continue below

Recommended for you

In my region it's tough to find fittings, pipe etc. in 304 or 316 that are NOT dual certified any more. Everybody's been stocking dual grade materials as the standard for at least the past 5+ years. Bar and plate are a different story, so product form matters a bit.

Dual certified materials meet the key requirements of both specs. 304/304L dual certified material has the strength to permit you to use the higher stress values for 304 material, while also meeting the low carbon spec of 304L grade for weldability.
 