Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Dsiposal of high content calcium chloride waters

Status
Not open for further replies.

asesor

Civil/Environmental
Aug 13, 2003
43
I have to dispose of 20.000 bbls of 40.000 ppm CaCl water. I dont have an injection well and would like to see if anybody has a better option than evaporation
Cost efficiency is also a must

 
Replies continue below

Recommended for you

Can't discharge to river or ocean? How about an evaporation Pond (if evaporation rate is higher than precipitation rate in your weather area)?

Ion exchange likely not a useful tool due to high concentrations already present.

Perhaps further concentration with electrodialysis or electrodialysis reversal, or reverse osmosis or pervaporation membrane? Then evaporate to dryness. Although, your stream is already rather concentrated.

Multiple effect evaporation system may be the best option. Expensive metallurgy, etc., but surprisingly efficient, at least when compared to just boiling water off in one stage. What else can one do and still obey laws of thermodynamics? It seems that this is what calcium chloride producers in the salt industry do.

Precipitate calcium as CaCO3? Even if possible at the high concentrations, Na2CO3 would surely need to be added, which would leave you with NaCl instead of CaCl .. not much further ahead? Total dissolved solids are not reduced.