What would be your favored material for piston rings in a compressor (dry) going to 10,000 psi or more? Gas is hydrogen.
 
Replies continue below

Recommended for you

Iainuts:

This will be a multi stage compressor.
In the low pressure stages you can use traditional materials.
In the high pressure stages ceramic materials work.