Jul 20, 2004 #1 barrney Industrial Joined Jul 20, 2004 Messages 1 Location US We are attempting to use a dry lube on a coil line. During humid weather the pinch rolls slip so that we don't get accurate feed lengths. Any suggestions or experience with this process and lube method?
We are attempting to use a dry lube on a coil line. During humid weather the pinch rolls slip so that we don't get accurate feed lengths. Any suggestions or experience with this process and lube method?
Jul 20, 2004 #2 gcaudill Electrical Joined Jan 20, 2003 Messages 180 Location US We put dry lube on wire. It's the very, very last step because of these types of problems. Will probably have to move lube or pinch rolls. Upvote 0 Downvote
We put dry lube on wire. It's the very, very last step because of these types of problems. Will probably have to move lube or pinch rolls.