We are drilling about 100 holes in some 4140A, .500 deep,.470 diam. No biggy right? We previously made these parts from 4140HT but were having problems pushing parts from the high cut force in milling and selected 4140A and will heat treat after.
Anyway, we previously drilled with HSS in a pinch and though slow, it worked decent but drills were paying the price. We decided to go for some carbide tipped drills and two toasted in 6 holes. Tips were chipped and one flute was cracked.
Here are the previous parameters. S1300, F6, Flood coolant, peck .200. We decided to go get some cobalt screw lengths to get it done but seems the decision on feeds/speeds varies greatly from SUPER ass slow, to slow with high feed.
I am not sure if we are really running into a work harden condition here or not but even at full hard, those carb drills should have hammered it. I guess I am not second guessing my plan. I was going to run the cobalts in the 60-80sf range and about .006/rev for starters. These are Morse split points, 135*, nothing special. Faster is always better but changing tools every 3rd part is not going to work either..
Anyway, we previously drilled with HSS in a pinch and though slow, it worked decent but drills were paying the price. We decided to go for some carbide tipped drills and two toasted in 6 holes. Tips were chipped and one flute was cracked.
Here are the previous parameters. S1300, F6, Flood coolant, peck .200. We decided to go get some cobalt screw lengths to get it done but seems the decision on feeds/speeds varies greatly from SUPER ass slow, to slow with high feed.
I am not sure if we are really running into a work harden condition here or not but even at full hard, those carb drills should have hammered it. I guess I am not second guessing my plan. I was going to run the cobalts in the 60-80sf range and about .006/rev for starters. These are Morse split points, 135*, nothing special. Faster is always better but changing tools every 3rd part is not going to work either..