COEngineeer
Structural
- Sep 30, 2006
- 1,186
So the county want a representative from the structural firm (me) and geotech at the site when they install these piers. The representative from the geotech. firm was there the whole day. I left after 4 pier installation. My question is, we specify to use (3)-#5 with ties at 48" o.c. We encountered some water in the hole so they decided to stick (3)-#5 without the ties so that you can lower the concrete pump hose all the way to the buttom so you can displace the water out. Is that common practice for residential construction? I was worried because how would we know that the rebars are lined up properly? The geotech guy told me it was ok. I didnt say anything because I felt that the geotech should be more in charge with the piers then I do. Comments?