We manufacture a small alum (5052-0) canister using a punch press and transfer tool. Part is ran at 40 pieces per minute. We then conveyor them to a standard cam driven lathe and C’Bore them. Note that the C’Bore is perpendicular to the press tool, or straight down stoke. The C’Bore is .287 +.003/-.000 x .175 +/-.002 deep.

Any advise on how this might be done in the Press transfer tool? Drill and Ream? And where I might find info on the required tooling?
Thanks!
 
Replies continue below

Recommended for you

Not recommended, mostly because both drill and ream tools produce chips, and piles of chips are not good for punch presses.