Jun 11, 2015 #1 Timbo1961 Automotive Joined Jan 24, 2013 Messages 9 Location GB Drill and Tap VS. Helicoil into Aluminium castings, debate
Jun 11, 2015 #2 MikeHalloran Mechanical Joined Aug 29, 2003 Messages 14,450 Location US Use the site's search feature; it will bury you in discussions. Mike Halloran Pembroke Pines, FL, USA Upvote 0 Downvote
Use the site's search feature; it will bury you in discussions. Mike Halloran Pembroke Pines, FL, USA
Jun 11, 2015 #3 Tmoose Mechanical Joined Apr 12, 2003 Messages 5,636 Location US Hi Timbo, What have you heard so far, to make you ask the question? Upvote 0 Downvote
Oct 28, 2015 #4 WernerQuevedo Automotive Joined Oct 28, 2015 Messages 4 Location IT If the part has to be put on and removed very few times, use aluminium, if it must be removed often, use helicoil. That's the rule we use for the racecar parts.Probably for different kind of cars this rule does not apply Upvote 0 Downvote
If the part has to be put on and removed very few times, use aluminium, if it must be removed often, use helicoil. That's the rule we use for the racecar parts.Probably for different kind of cars this rule does not apply