Sep 27, 2019 #1 VigneshK Mechanical Joined Jun 29, 2018 Messages 7 Location AE Dear expertise. I Need know what is the minimum distance of drawoff sump outer ring weld to bottom plate lap weld?
Dear expertise. I Need know what is the minimum distance of drawoff sump outer ring weld to bottom plate lap weld?
Sep 27, 2019 #2 JStephen Mechanical Joined Aug 25, 2004 Messages 8,729 Location US As far as I know, there is no minimum, seams can cross the sump. That's undesirable for fit-up and welding, but not prohibited. Upvote 0 Downvote
As far as I know, there is no minimum, seams can cross the sump. That's undesirable for fit-up and welding, but not prohibited.