Hello Everybody,

I have a LEMO B type connector (FGG.0B). This is the first time I am working this, so my question is quite basic. How do I connect the wires to the pins, which are in the shape of the eyebrow or half moon shaped. I have read a ew instruction in below link, however it does not explicitly talks about soldering, however there are certain parameters mentioned for the soldering.


Thanks and I appreciate your help,
Padmanapan
 
Replies continue below

Recommended for you

That connector has either crimp or solder contacts..
Which did you get?
 
lemo_pin_agleey.png


I am pretty sure it is a soldering contact after going through slide# 11 in the website from where I have also uploaded an Image. It calls it as a soldering joint, so I assume it needs to be soldered.

Is there a specific way to solder this contact, could please suggest me link I can look for soldering methods for this, or it is just the conventional way.

Thanks once again
Padmanapan
 